Factors that Cause Battery Deterioration

Under Charging
The signs are as follows:
- white stain is formed on the plates, making it difficult to charge the electricity
- Plates will also erode
Over Charging
The signs are as follows:
- A large amount of distilled water transforms into gas, causing the level to distilled water to drop significantly
- Temperature rises, causing plates to deteriorate
- Erosion of lead powder as a result of plate deterioration
- Erosion of lead powder as a result of plate deterioration
- Battery life is shortened
Short Circuit
The signs are as follows:
- Too much sediment left at the bottom of the battery box
- The separator between positive and negative plates may be broken into pieces or deteriorate
Problem with the Electrical System
The signs are as follows:
- Installation of additional systems such as stereo system, theft prevention system and other accessories, which may cause insufficient amount of electricity
- Changes in the battery size
- Short circuit of several electric switches in the car
- The alternator is not working efficiently
Impurity in the battery box
The signs are as follows:
- Quality of electrolyte is not up to standard
- Distilled water is not pure enough
- Coolant has been added
Sulfation
White sulfuric stain on the plates appears as a result of:
- The battery is being abandoned for a long time
- Under charging
- Plate emerges above electrolyte level

Copyright 2019 All right reserved B-Quik.com